Images are for guidance only and might not represent the final product.
Formula: Co 49/Fe 49/V 2
Form: Rod
Material: Permendur® 49
Commodity: Alloys
Hazard Pictogram: GHS07, GHS08
Permendur® 49 Rods are made from an iron-cobalt alloy known for its high saturation induction and low coercivity, making it useful in applications like electric motors, transformers, and magnetic shields. With 79 size variations in the range, our Permendur® 49 Rods allow flexibility in design and integration into diverse systems and components. It is used primarily as magnetic core material in electrical core material in electrical equipment requiring high permeability values at very high magnetic flux densities, such as lightweight transformers and electric motors.
Technical Data Sheet Safety Data Sheet Tolerance Properties

Health hazard/Hazardous to the ozone layer

Serious health hazard

each

We are collecting your products, please wait!...

Shipping restrictions and charges
may apply for some hazardous materials.

Tolerances

Rod
Diameter =<10mm ±10%
Diameter >10mm ±5%

Material Properties for Alloys

Mechanical Properties
Element Value
Elongation at break( % ) 6
Electrical Properties
Element Value
Electrical resistivity( µOhmcm ) 40
Magnetic Properties
Element Value
Curie temperature( C ) 940
Saturation flux density( T ) 2.34
Physical Properties
Element Value
Density( gcm⁻³ ) 8.15
Thermal Properties
Element Value
Coefficient of thermal expansion( x10⁻⁶ K⁻¹ ) 9.5@20°C