Grade: Inconel® 625
Formula: Ni61/Cr22/Mo 9/Fe 5
Form: Rod
Material: Inconel®
Commodity: Alloys
Temper: Annealed
Inconel® 625 Rod is a nickel–chromium–molybdenum alloy that provides outstanding resistance to oxidation, fatigue, and chloride stress corrosion cracking while offering high tensile and creep strength across a broad temperature range. In rod form, it delivers structural stability and machinability, making it indispensable in aerospace, marine, and chemical industries. Primary applications include turbine shafts, reactor supports, and marine fasteners where long-term performance under corrosive and thermally demanding conditions is essential. Specific uses extend to welded components for chemical plants, bearing parts in propulsion systems, and structural rods in nuclear facilities. Research has investigated its tribological behavior with micro-textures to enhance wear resistance, grain evolution during thermal aging and HIP processing, and weldability optimization through laser beam welding, demonstrating its adaptability for high-performance environments. By combining mechanical durability, corrosion resistance, and processing flexibility, Inconel® 625 Rod proves its continued importance for scientific advancements and industrial innovation.

Health hazard/Hazardous to the ozone layer

Serious health hazard

each

We are collecting your products, please wait!...

Shipping restrictions and charges
may apply for some hazardous materials.

Tolerances

Rod
Diameter =<10mm ±10%
Diameter >10mm ±5%

Material Properties for Alloys

Mechanical Properties
Element Value
Hardness - Brinell 175-240
Elongation at break( % ) <40
Modulus of elasticity( GPa ) 147-210
Tensile strength( MPa ) 950
Magnetic Properties
Element Value
Initial permeability 1.0006
Curie temperature( C ) -196
Electrical Properties
Element Value
Electrical resistivity( µOhmcm ) 129
Temperature coefficient( K⁻¹ ) -
Thermal Properties
Element Value
Melting point( C ) 1290-1350
Specific heat( J K⁻¹ kg⁻¹ ) 410@23°C
Thermal conductivity( W m⁻¹ K⁻¹ ) 9.8@23°C
Coefficient of thermal expansion( x10⁻⁶ K⁻¹ ) 12.8@20-100°C
Physical Properties
Element Value
Density( gcm⁻³ ) 8.44