Grade: Inconel® 617
Formula: Ni 57/Cr 22/Co 12/Mo 9
Form: Rod
Material: Nickel/Chromium (Inconel®)
Commodity: Alloys
Temper: Annealed
Inconel® 617 Rod is a nickel–chromium–cobalt–molybdenum alloy developed for high-temperature strength and resistance to both oxidation and carburization. Its rod form provides excellent mechanical integrity, machinability, and durability in structural applications requiring stability under extreme heat and stress. It is widely employed in aerospace, power generation, and petrochemical industries, particularly in turbine components, furnace supports, and reformer systems. Specific uses include combustion chamber hardware in gas turbines, welded components in high-temperature reactors, and structural parts for chemical plants requiring long-term creep and fatigue resistance. Research has explored its fatigue life under thermo-mechanical stress, its weldability and microstructural transformations during TIG welding, and optimization of protective coatings to further enhance surface performance. With its superior strength retention at elevated temperatures and adaptability to advanced fabrication processes, Inconel® 617 Rod stands as a cornerstone material for both scientific advancements and industrial innovation.

Health hazard/Hazardous to the ozone layer

Serious health hazard

each

We are collecting your products, please wait!...

Shipping restrictions and charges
may apply for some hazardous materials.

Tolerances

Rod
Diameter =<10mm ±10%
Diameter >10mm ±5%

Material Properties for Alloys

Mechanical Properties
Element Value
Elongation at break( % ) 62
Modulus of elasticity( GPa ) 190-200
Izod impact strength( J m⁻¹ ) 232
Tensile strength( MPa ) 730-760
Electrical Properties
Element Value
Electrical resistivity( µOhmcm ) 1.22-1.34
Temperature coefficient( K⁻¹ ) -
Thermal Properties
Element Value
Melting point( C ) 1332-1380
Specific heat( J K⁻¹ kg⁻¹ ) 419@23°C
Thermal conductivity( W m⁻¹ K⁻¹ ) 13.4@23°C
Coefficient of thermal expansion( x10⁻⁶ K⁻¹ ) 11.6@20-200°C
Physical Properties
Element Value
Density( gcm⁻³ ) 8.36

Can't find what you're looking for? For customized options