Images are for guidance only and might not represent the final product.

Hastelloy® C-276 Rod

Available Configurations

Properties common to all products in this list

Grade: Hastelloy® C-276 Composition: Ni 57/Mo 17/Cr 16/Fe/W/Mn Form: Rod Material: Nickel/Molybdenum (Hastelloy®) UNS Number: N10276 Commodity: Alloys
Hastelloy® C-276 Rod is a high-performance nickel-chromium-molybdenum alloy rod widely recognized for its resistance to strong oxidizing and reducing conditions, making it invaluable across aerospace, chemical processing, and nuclear industries. Its robust mechanical strength at elevated temperatures, combined with corrosion resistance, allows precise machining and shaping into components for extreme environments. The rod form is particularly suited to structural applications and experimental studies where uniformity and durability are critical. Specific technologies benefiting from Hastelloy® C-276 rods include sustainable machining under dry, flood, and minimum quantity lubrication (MQL) conditions, where optimized cooling reduces cutting forces, energy consumption, and tool wear; forging processes designed to reduce grain boundary embrittlement and prevent cracking during high-temperature forming; and predictive machining models using fuzzy logic for estimating cutting forces and optimizing process parameters. In research, rods serve as test specimens for mechanical, thermal, and corrosion evaluations, advancing understanding of superalloy behavior under complex stresses. By uniting strength, corrosion resistance, and fabrication adaptability, Hastelloy® C-276 Rod continues to provide unmatched value in both scientific development and industrial innovation.

Health hazard/Hazardous to the ozone layer

Serious health hazard

Starting at $189.00 each
No Minimum order Free technical support *Free delivery worldwide

Material Properties

Mechanical Properties
Element Value
Hardness - Brinell 80-200
Elongation at break( % ) 52
Modulus of elasticity( GPa ) 170-220
Izod impact strength( J m⁻¹ ) 42-100
Tensile strength( MPa ) 550-900
Electrical Properties
Element Value
Electrical resistivity( µOhmcm ) 125-130
Thermal Properties
Element Value
Maximum use temperature in air( C ) 1090
Melting point( C ) 1270-1390
Specific heat( J K⁻¹ kg⁻¹ ) 427@23°C
Thermal conductivity( W m⁻¹ K⁻¹ ) 10.1-12.5@23°C
Coefficient of thermal expansion( x10⁻⁶ K⁻¹ ) 10.8-11.3@20-100
Physical Properties
Element Value
Density( gcm⁻³ ) 8.94
each

Choose Your Options

Close

Available Configurations

Properties common to all products in this list

Grade: Hastelloy® C-276 Composition: Ni 57/Mo 17/Cr 16/Fe/W/Mn Form: Rod Material: Nickel/Molybdenum (Hastelloy®) UNS Number: N10276 Commodity: Alloys

We are collecting your products, please wait!...

Shipping restrictions and charges may apply for some hazardous materials.

Tolerances

Rod
Diameter =<10mm ±10%
Diameter >10mm ±5%
Length <100mm ±1mm
Length >=100mm +5 / -1%