Images are for guidance only and might not represent the final product.
Grade: Monel® 400
Formula: Ni 65/Cu 33/Fe 2
Form: Coil
Material: Nickel/Copper (Monel®)
Commodity: Alloys
Temper: Annealed
Monel® 400 Coil is a nickel-copper alloy coil recognized for its exceptional resistance to seawater corrosion, acids, and alkalis, while also offering excellent mechanical strength and toughness across a wide temperature range. The coil form enhances flexibility in manufacturing and makes it particularly suited for producing long-length tubing and components for demanding industrial uses. It finds primary applications in marine engineering, chemical processing, and nuclear power systems where both structural reliability and corrosion resistance are paramount. Specifically, Monel® 400 coils are used in heat exchanger tubing, pump and valve components, and process equipment that must withstand harsh, corrosive fluids. In research and development, this alloy continues to be explored for its weldability, machinability, and adaptability in advanced joining and forming technologies. Its role as a coil-based material not only facilitates high-efficiency production but also ensures long-term durability, cementing its importance in both scientific study and industrial deployment across sectors where material integrity cannot be compromised.

Health hazard/Hazardous to the ozone layer

Serious health hazard

each

We are collecting your products, please wait!...

Shipping restrictions and charges
may apply for some hazardous materials.

Tolerances

Coil
Thickness <0.01mm ±25%
Thickness 0.01mm - 0.05mm ±15%
Thickness >0.05mm ±10%

Material Properties for Alloys

Mechanical Properties
Element Value
Hardness - Brinell 125-190
Elongation at break( % ) <40
Modulus of elasticity( GPa ) 185
Izod impact strength( J m⁻¹ ) 110-140
Tensile strength( MPa ) 550-950
Electrical Properties
Element Value
Electrical resistivity( µOhmcm ) 48-51
Temperature coefficient( K⁻¹ ) 0.0019
Thermal Properties
Element Value
Maximum use temperature in air( C ) 450
Melting point( C ) 1300-1350
Thermal conductivity( W m⁻¹ K⁻¹ ) 21.7@23°C
Coefficient of thermal expansion( x10⁻⁶ K⁻¹ ) 13.9-14.1@20-100°C
Physical Properties
Element Value
Density( gcm⁻³ ) 8.84

Can't find what you're looking for? For customized options