Images are for guidance only and might not represent the final product.
Grade: Hastelloy® C-276
Formula: Ni 57/Mo 17/Cr 16/Fe/W/Mn
Form: Coil
Material: Hastelloy®
Commodity: Alloys
Hastelloy® C-276 Coil is a nickel-chromium-molybdenum alloy supplied in coiled sheet form, offering excellent resistance to both oxidizing and reducing media. Known for its resilience against strong chlorides, wet chlorine gas, and oxidizing salts, it is widely employed in chemical processing, marine engineering, and environmental systems. The coiled geometry provides versatility in fabrication, making it suitable for cladding, lining, and forming corrosion-resistant components. Specific technologies benefiting from Hastelloy® C-276 coil include electrochemical micromachining (µECM), where it provides stable performance for micro-hole drilling with optimized electrolytes; high-temperature aging studies that reveal its resistance to precipitation-induced sensitization while retaining corrosion resistance in chloride environments; and machining research showing its durability under both dry and wet milling conditions, enabling precise manufacturing of high-integrity components. In research and industry, Hastelloy® C-276 coils are indispensable for developing advanced corrosion-resistant systems, ensuring reliable long-term operation in aggressive environments. By combining formability, corrosion resistance, and adaptability, Hastelloy® C-276 Coil remains vital to innovation across multiple sectors.

Health hazard/Hazardous to the ozone layer

Serious health hazard

each

We are collecting your products, please wait!...

Shipping restrictions and charges
may apply for some hazardous materials.

Tolerances

Coil
Thickness <0.01mm ±25%
Thickness 0.01mm - 0.05mm ±15%
Thickness >0.05mm ±10%

Material Properties for Alloys

Mechanical Properties
Element Value
Hardness - Brinell 80-200
Elongation at break( % ) 52
Modulus of elasticity( GPa ) 170-220
Izod impact strength( J m⁻¹ ) 42-100
Tensile strength( MPa ) 550-900
Electrical Properties
Element Value
Electrical resistivity( µOhmcm ) 125-130
Thermal Properties
Element Value
Maximum use temperature in air( C ) 1090
Melting point( C ) 1270-1390
Specific heat( J K⁻¹ kg⁻¹ ) 427@23°C
Thermal conductivity( W m⁻¹ K⁻¹ ) 10.1-12.5@23°C
Coefficient of thermal expansion( x10⁻⁶ K⁻¹ ) 10.8-11.3@20-100
Physical Properties
Element Value
Density( gcm⁻³ ) 8.94