Grade: Grade 1
Formula: Ti
Form: Rod
Material: Titanium
CAS Number: 7440-32-6
Commodity: Metals
Purity: 99.6%
Temper: Annealed
Grade 1 Titanium Rod is a commercially pure titanium product known for its highest ductility and formability among unalloyed grades, with excellent corrosion resistance and service capability from –184 °C to 540 °C. It combines low tensile strength with superior cold workability and is often selected for its 99.6% purity. It finds widespread application across marine engineering, chemical processing, desalination, and biomedical fields. Key use cases include deep-drawn heat exchanger plates, seawater-cooled condenser tubes, complex-shaped corrosion-resistant parts, and surface-protective cladding layers in biocompatible implants. Its low density and thermal compatibility with carbon steel also make it ideal for weight-sensitive and thermally fluctuating systems. Grade 1 Titanium Rod plays a pivotal role in R&D of laser-induced surface strengthening, corrosion immunity studies in polluted waters, and fatigue resistance in lightweight structural assemblies. Its outstanding formability and long-term stability in extreme conditions underscore its continued scientific and industrial relevance.
each

We are collecting your products, please wait!...

Shipping restrictions and charges
may apply for some hazardous materials.

Tolerances

Rod
Diameter =<10mm ±10%
Diameter >10mm ±5%

Material Properties for Metals

Atomic Properties
Element Value
Atomic number 22
Crystal structure Hexagonal close packed
Electronic structure Ar 3d² 4s²
Valences shown 2,3,4
Atomic weight( amu ) 47.88
Thermal neutron absorption cross-section( Barns ) 6.1
Photo-electric work function( eV ) 4.1
Natural isotope distribution( Mass No./% ) 50/ 5.3
Natural isotope distribution( Mass No./% ) 49/ 5.5
Natural isotope distribution( Mass No./% ) 46/ 8.0
Natural isotope distribution( Mass No./% ) 48/ 73.7
Natural isotope distribution( Mass No./% ) 47/ 7.5
Atomic radius - Goldschmidt( nm ) 0.147
Ionisation potential( No./eV ) 3/ 27.5
Ionisation potential( No./eV ) 4/ 43.3
Ionisation potential( No./eV ) 5/ 99.2
Ionisation potential( No./eV ) 1/ 6.82
Ionisation potential( No./eV ) 2/ 13.6
Ionisation potential( No./eV ) 6/ 119
Mechanical Properties
Element Value
Material condition Polycrystalline
Material condition Annealed
Poisson's ratio 0.361
Poisson's ratio 0.361
Poisson's ratio -
Bulk modulus( GPa ) 108.4
Bulk modulus( GPa ) -
Bulk modulus( GPa ) 108.4
Tensile modulus( GPa ) -
Tensile modulus( GPa ) 120.2
Tensile modulus( GPa ) 120.2
Izod toughness( J m⁻¹ ) 61
Izod toughness( J m⁻¹ ) 61
Hardness - Vickers( kgf mm⁻² ) 60
Hardness - Vickers( kgf mm⁻² ) 60
Tensile strength( MPa ) 230-460
Tensile strength( MPa ) 230-460
Yield strength( MPa ) 140-250
Yield strength( MPa ) 140-250
Electrical Properties
Element Value
Electrical resistivity( µOhmcm ) 54@20@20°C
Superconductivity critical temperature( K ) 0.4
Temperature coefficient( K⁻¹ ) 0.0038@0-100°C
Physical Properties
Element Value
Boiling point( C ) 3287
Density( gcm⁻³ ) 4.5@20°C
Thermal Properties
Element Value
Melting point( C ) 1660
Latent heat of evaporation( J g⁻¹ ) 8893
Latent heat of fusion( J g⁻¹ ) 365
Specific heat( J K⁻¹ kg⁻¹ ) 523@25°C
Thermal conductivity( W m⁻¹ K⁻¹ ) 21.9@0-100°C
Coefficient of thermal expansion( x10⁻⁶ K⁻¹ ) 8.9@0-100°C