Polyphenylenesulfide - 20% Carbon Fiber Reinforced ( PPS - 20% CFR )

Material Information

Buy Polyphenylenesulfide - 20% Carbon Fiber Reinforced on-line

We stock and supply the following standard forms:
Granule
Granule

Choose a form to search our on-line catalog  

Chemical Resistance

Acids - concentrated Fair
Acids - dilute Good
Alcohols Good
Alkalis Good
Aromatic hydrocarbons Good
Greases and Oils Good
Halogens Fair
Ketones Good

Electrical Properties

Surface resistivity ( Ohm/sq ) 103
Volume resistivity ( Ohmcm ) 103

Mechanical Properties

Elongation at break ( % ) 2
Izod impact strength ( J m-1 ) 53
Tensile modulus ( GPa ) 17
Tensile strength ( MPa ) 180

Physical Properties

Density ( g cm-3 ) 1.41
Flammability V-0
Water absorption - over 24 hours ( % ) <0.05

Thermal Properties

Coefficient of thermal expansion ( x10-6 K-1 ) 15
Heat-deflection temperature - 1.8MPa ( C ) 260
Thermal conductivity @0.47C ( W m-1 K-1 )
Upper working temperature ( C ) 220